Before construction:
1. Add 5% -20% distilled water and stir evenly before applying. This product can be applied by brushing, wiping, rolling, high-pressure airless spraying, or combined with other equipment.
2. The construction environment temperature should be above the dew point: 5 ℃ -80 ℃, humidity should be below 85%, and construction cannot be carried out outdoors on rainy or snowy days.
3. Remove dust, dirt, and debris from the surface of the substrate before application, and keep the working surface dry.
During construction:
4. Use the cross roll coating method or cross spray coating method to continuously construct the color steel tile roof, spraying twice with an interval of 2 hours.
5. The coating construction is carried out from top to bottom of the building, and each spraying or rolling coating is divided by natural dividing joints, internal and external corner junctions, or downspouts. Each coating surface should be completed as much as possible in one go.
6. During construction, the coating should be evenly applied, without exposing the base or sagging, and the color should be consistent.
After construction:
7. Coating products should be stored in a cool environment, and the recommended long-term storage temperature is between 5-30 ℃.
During transportation, long-term exposure to sunlight, collisions, and heavy pressure should be avoided as much as possible to maintain the integrity of the packaging.